Kuhn and Persistence Length of Polymers

Polymer lK (nm) lP (nm)
Polyethylene 1.2 2.6
Polypropylene 1.1 2.3
syndiotactic. Polypropylene 1.7 3.4
isotactic Polypropylene 1.1 2.3
Poly(1-butene) 1.1 2.2
Polyisobutylene 1.2 2.5
cis- Polyisoprene 0.9 1.9
cis-Polybutadiene 0.8 1.7
Polymethylacrylate 1.5 2.9
Polyethylacrylate 1.8 3.6
Polymethylmethacrylate 1.5 3.1
Polyhexylmethacrylate 2.4 4.9